ʻO ka hana nui o MOS2 i hoʻohana ʻia no nā mea friction e hoʻemi i ka friction i ka haʻahaʻa haʻahaʻa a hoʻonui i ka friction ma ke kiʻekiʻe wela. He liʻiliʻi ka nalowale o ka puhi ʻana i nā mea friction.
ʻO ka hoʻohaʻahaʻa haʻahaʻa: ʻo ka nui o ka MOS2 i hana ʻia e ka luku ʻana i ka ea supersonic a hiki i ka 325-2500 mesh, ʻo ka paʻakikī o nā micro particles he 1-1.5, a ʻo ka friction coefficient he 0.05-0.1. No laila, hiki iā ia ke pāʻani i ka hoʻemi friction i nā mea friction.
Rammerization: ʻAʻole alakaʻi ʻo MOS2 i ka uila a aia kahi copolymer o MOS2, MOS3 a me MoO3. Ke piʻi ikaika ka mahana o ka mea friction ma muli o ka friction, hoʻonui ʻia nā ʻāpana MoO3 i loko o ka copolymer me ka piʻi ʻana o ka mahana, e pāʻani ana i kahi kuleana o ka friction.
Anti-oxidation: Loaʻa ka MOS2 ma o ka hoʻomaʻemaʻe hoʻomaʻemaʻe ʻana i ka hoʻohuihui; ʻO kona PH waiwai he 7-8, alkaline iki. Uhi ia i ka ʻili o ka mea friction, hiki ke pale i nā mea ʻē aʻe, pale iā lākou mai ka oxidized, ʻoi aku ka maʻalahi o ka hāʻule ʻana o nā mea ʻē aʻe, hoʻonui ʻia ka ikaika adhesion.
ʻO ka maikaʻi: 325-2500 mesh;
PH: 7-8; Ka nui: 4.8 a i ka 5.0 g/cm3; Ka paakiki: 1-1.5;
Hoʻopau i ka hoʻopau ʻana: 18-22%;
ʻO ke koena hoʻoheheʻe: 0.05-0.09
Hoʻohana nui ʻia i nā mīkini, nā mea kani, nā ʻāpana kaʻa, ka uila a me ka uila, ke kaʻaahi, nā mea hana hale, nā kamaʻilio, nā mīkini textile, nā haʻuki a me nā huahana leʻaleʻa, nā paipu aila, nā pahu wahie a me nā huahana ʻenekinia pololei.
Kahua | Nā hihia noi |
Nā lako uila | ʻO ke kukui uila, laser, photoelectric detector, |
Nā ʻāpana uila & uila | Mea hoʻohui, bobbin, timer, uhi kaapuni, hoʻololi hale |